Hot Cracking of Nickel-Based Superalloy Turbine Blade
Metallurgy and Foundry Engineering
doi 10.7494/mafe.2015.41.4.181
Full Text
Open PDFAbstract
Available in full text
Date
January 1, 2015
Authors
Publisher
AGHU University of Science and Technology Press