Final Report - LAW Envelope a and B Glass Formulations Testing in Increase Waste Loading. VSL-06R6900-1

doi 10.2172/1109497
Full Text
Open PDF
Abstract

Available in full text

Date

December 3, 2013

Authors
Albert A. KrugerI. JosephI. S. MullerW. GongH. GanI. L. PeggK. S. Matlack
Publisher

Office of Scientific and Technical Information (OSTI)


Related search

Final Report - Melt Rate Enhancement for High Aluminum HLW Glass Formulation, VSL-08R1360-1, Rev. 0, Dated 12/19/08

2013English

Development of High Waste-Loading HLW Glasses for High Bismuth Phosphate Wastes, VSL-12R2550-1, Rev 0

2012English

Melt Rate Enhancement for High Aluminum HLW (High Level Waste) Glass Formulation Final Report 08r1360-1

2010English

Studies and Testing of Antireflective (AR) Coatings for Soda-Lime Glass. Final Report

1978English

Final Report - Management of High Sulfur HLW, VSL-13R2920-1, Rev. 0, Dated 10/31/2013

2013English

Effects of Tuff Waste Package Components on Release From 76-68 Simulated Waste Glass: Final Report

1984English

Final Report Integrated Dm1200 Melter Testing Using Az 102 and C 106/Ay-102 HLW Simulants: HLW Simulant Verification VSL-05r5800-1 Rev 0 6/27/05

2011English

Testing of Organic Waste Surrogate Materials in Support of the Hanford Organic Tank Program. Final Supplementary Report, Supplement 1

1994English

Vaccine Refrigerator Testing. Final Report

1990English

Amanote Research

Note-taking for researchers

Follow Amanote

© 2025 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy