Study on Galvanic Corrosion and Its Prevention in Building Piping System

Journal of Architecture and Planning (Transactions of AIJ)
doi 10.3130/aija.61.51_5
Full Text
Open PDF
Abstract

Available in full text

Date

January 1, 1996

Authors
Toshihiro YAMATETatsuya YOSHIDAKatuji TUZUKISatoru KANEKO
Publisher

Architectural Institute of Japan


Related search

Galvanic Corrosion Study on Stainless Steel Cartridge Design

2008English

Galvanic Corrosion Studies on Titanium and Zirconium Metals

1954English

Corrosion and Its Prevention for Oil Tankers

Journal of Zosen Kiokai
1961English

Galvanic Corrosion in Oil and Gas Well Fluids

Corrosion Engineering
Materials ScienceEngineering
1954English

Galvanic Corrosion Behavior of Dental Alloys

2012English

Case Study on the Bluish Water Phenomenon in Copper Piping System

Journal of Environmental Engineering (Japan)
Environmental Engineering
2005English

Erratum to : Galvanic Corrosion in Oil and Gas Well Fluids

Corrosion Engineering
Materials ScienceEngineering
1954English

Galvanic Corrosion of Lithium‐Powder‐Based Electrodes

Advanced Energy Materials
Materials Sciencethe EnvironmentSustainabilityRenewable Energy
2020English

Corrosion Fatigue Crack Growth Studies on Pressure Vessel and Piping Steels in Water Environment

Archives of Metallurgy and Materials
2017English

Amanote Research

Note-taking for researchers

Follow Amanote

© 2026 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy