Atomic Layer Deposition of Ultrathin Copper Metal Films From a Liquid Copper(I) Amidinate Precursor
Journal of the Electrochemical Society - United States
doi 10.1149/1.2338632
Full Text
Open PDFAbstract
Available in full text
Categories
Date
January 1, 2006
Authors
Publisher
The Electrochemical Society