Structure/Property Interactions in a Long Range Order Strengthened Superalloy

doi 10.7449/2000/superalloys_2000_553_562
Full Text
Open PDF
Abstract

Available in full text

Date

January 1, 2000

Authors
M.F. RothmanD.L. KlarstromM. DollarJ.F. Radavich
Publisher

TMS


Related search

Long-Range Chromatin Interactions

Cold Spring Harbor perspectives in biology
BiochemistryGeneticsMolecular Biology
2015English

Long-Range Chromatin Interactions in the Kidney

Journal of the American Society of Nephrology : JASN
MedicineNephrology
2019English

Short Range Smectic Order Driving Long Range Nematic Order: Example of Cuprates

Scientific Reports
Multidisciplinary
2016English

Long Range Interactions in Magneto-Optical Traps

AIP Conference Proceedings
AstronomyPhysics
2008English

Partial Long-Range Order in Antiferromagnetic Potts Models

Physical Review B
2014English

Long-Range Interactions of Lithium Atoms

Physical Review A
1997English

Abnormal Grain Growth in Oxide Dispersion Strengthened Ni-Base Superalloy

Materials Transactions, JIM
1992English

Long-Range Interactions in Antiferromagnetic Quantum Spin Chains

Physical Review B
OpticalElectronicCondensed Matter PhysicsMagnetic Materials
2017English

Epigenetics of Long-Range Chromatin Interactions

Pediatric Research
Child HealthPediatricsPerinatology
2007English

Amanote Research

Note-taking for researchers

Follow Amanote

© 2026 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy