Nanoindentation-Induced Deformation Behavior in the Vicinity of Single Grain Boundary of Interstitial-Free Steel

Materials Transactions - Japan
doi 10.2320/matertrans.46.2026
Full Text
Abstract

Available in full text

Date
Authors
Publisher