Effects of Corrosion Environments on Stress Corrosion Cracking of Al-Zn-Mg Alloys
Keikinzoku/Journal of Japan Institute of Light Metals - Japan
doi 10.2464/jilm.20.331
Full Text
Open PDFAbstract
Available in full text
Date
January 1, 1970
Authors
Publisher
Japan Institute of Light Metals