Amanote Research

Amanote Research

    RegisterSign In

Ten-Year Creep Test of Tage Tuff

Journal of MMIJ
doi 10.2473/journalofmmij.124.741
Full Text
Open PDF
Abstract

Available in full text

Date

January 1, 2008

Authors
Kimihiro HASHIBASeisuke OKUBOKatsunori FUKUI
Publisher

Mining and Materials Processing Institute of Japan


Related search

Long-Term Creep Test and Constitutive Equation of Tage Tuff.

Shigen-to-Sozai
2002English

The Ten-Year Plan

Econometrica
EconomicsEconometrics
1961English

Modeling of a Modified Rocha Slot Test in Welded Tuff

1987English

Ten-Year Anniversary of CD3δ Deficiency

LymphoSign Journal
2015English

Blasse Tage

Sirena: poesia, arte y critica
2010English

A Simple Constant Stress Creep Test

JOM
Materials ScienceEngineering
1949English

Evaluation of Creep Properties of Reduced Activation Ferritic Steels by Small Punch Creep Test

Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals
Mechanics of MaterialsAlloysMaterials ChemistryCondensed Matter PhysicsMetals
2006English

Ten-Year Celebration of the Declaration of Istanbul

American Journal of Transplantation
TransplantationAllergyImmunologyPharmacology
2018English

Management of Acute Osteomyelitis: A Ten-Year Experience

Infectious Disease Reports
Infectious Diseases
2016English

Amanote Research

Note-taking for researchers

Follow Amanote

© 2026 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy