Comparative Study of the Wear Resistance of Al2O3-Coated MA956 Superalloy

Revista de Metalurgia- Spain

doi 10.3989/revmetalm.2000.v36.i5.583

Full Text

Abstract

Available in

Date

Authors

Publisher

Editorial CSIC


Related search