Inverse Analysis of Galvanic Corrosion Problems Using Fuzzy Apriori Information.

Transactions of the Japan Society of Mechanical Engineers Series A
doi 10.1299/kikaia.59.1562
Full Text
Open PDF
Abstract

Available in full text

Date

January 1, 1993

Authors
Shigeru AokiKenji AmayaJun Togashi
Publisher

Japan Society of Mechanical Engineers


Related search

Galvanic Corrosion Behavior of Dental Alloys

2012English

On the Solution of Inverse Problems With Fuzzy Correspondences

2019English

Robustness Analysis for Scheduling Problems Using the Inverse Method

2012English

Galvanic Corrosion of Lithium‐Powder‐Based Electrodes

Advanced Energy Materials
Materials Sciencethe EnvironmentSustainabilityRenewable Energy
2020English

Bayesian Analysis in Inverse Problems

Inverse Problems
Mathematical PhysicsApplied MathematicsComputer Science ApplicationsSignal ProcessingTheoretical Computer Science
1991English

Development of Effective BEM for Galvanic Corrosion Analysis of a Slender Structure.

Transactions of the Japan Society of Mechanical Engineers Series A
1992English

Galvanic Corrosion of Duplex Corrosion-Resistant Steel Rebars Under Carbonated Concrete Conditions

RSC Advances
ChemistryChemical Engineering
2018English

Galvanic Corrosion Study on Stainless Steel Cartridge Design

2008English

Galvanic Corrosion Studies on Titanium and Zirconium Metals

1954English

Amanote Research

Note-taking for researchers

Follow Amanote

© 2026 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy