Volume Variation Process of High-Density Polyethylene During Tensile and Creep Tests
Oil and Gas Science and Technology - France
doi 10.2516/ogst:2006009
Full Text
Open PDFAbstract
Available in full text
Date
November 1, 2006
Authors
Publisher
EDP Sciences