Study of 2D and 3D Methods for Worn Surface Analysis of Tool Materials

Acta Technica Jaurinensis
doi 10.14513/actatechjaur.v8.n2.373
Full Text
Open PDF
Abstract

Available in full text

Date

April 30, 2015

Authors
I. HatosH. HargitaiL. Solecki
Publisher

Faculty of Mechanical Engineering, Informatics and Electrical Engineering


Related search

Quantitative Posture Analysis of 2D, 3D, and Optical Microscope Visualization Methods for Microsurgery Tasks

Work
MedicineEnvironmentalPublic HealthRehabilitationOccupational Health
2012English

Analysis of Worn Surfaces of Polymeric Materials

NIPPON GOMU KYOKAISHI
2007English

Efficient High-Resolution Surface Patterning for 2D and 3D Parts

SPIE Newsroom
2016English

“Gold Standard” Data for Evaluation and Comparison of 3d/2d Registration Methods

Computer Aided Surgery
2004English

Topological Analysis and Symbol for 2d- And 3d-Networks

Nihon Kessho Gakkaishi
2016English

A Facile Route for 3D Aerogels From Nanostructured 1D and 2D Materials

Scientific Reports
Multidisciplinary
2012English

3D Surface Configuration Modulated 2D Symmetry Detection

i-Perception
OphthalmologySensory SystemsExperimentalArtificial IntelligenceCognitive Psychology
2011English

Applying 2D Shape Analysis Techniques to Granular Materials With 3D Particle Geometries

2009English

Measuring Surface Area of Skin Lesions With 2D and 3D Algorithms

International Journal of Biomedical Imaging
Nuclear MedicineRadiologyImaging
2019English

Amanote Research

Note-taking for researchers

Follow Amanote

© 2026 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy