On Chemical and Diffusional Interactions Between PCBN and Superalloy Inconel 718: Imitational Experiments
Journal of the European Ceramic Society - Netherlands
doi 10.1016/j.jeurceramsoc.2019.03.002
Full Text
Open PDFAbstract
Available in full text
Date
July 1, 2019
Authors
Publisher
Elsevier BV