Generation and Propagation of Intergranular Stress Corrosion Cracks of Sensitized SUS304 Stainless Steel in NaF Aqueous Solution

Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan - Japan
doi 10.2355/tetsutohagane1955.79.6_726