In Situ Diagnostics of Damage Accumulation in Ni-Based Superalloys Using High-Temperature Computed Tomography

Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science - United States
doi 10.1007/s11661-018-4737-6
Full Text
Abstract

Available in full text

Date
Authors
Publisher

Springer Science and Business Media LLC