Precipitated Phases and Weld Crackings of Nickel-Base Superalloys

Yosetsu Gakkai Shi/Journal of the Japan Welding Society- Japan

doi 10.2207/qjjws1943.38.9_979

Full Text

Abstract

Available in

Categories

Mechanics of MaterialsSurfacesAlloysMechanical EngineeringMetalsFilmsCoatings

Date

January 1, 1969

Authors

Hiroshi Ikawa

Publisher

Japan Welding Society


Related search

Formation of Topologically Closed Packed Phases in Nickel Base Single Crystal Superalloys

1988English

Oxidation of Nickel and Cobalt-Base Superalloys

1965English

Alloy Design of Nickel-Base Precipitation Hardened Superalloys

Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan
AlloysCondensed Matter PhysicsMetalsTheoretical ChemistryMaterials ChemistryPhysical
1975English

Microstructural Stability and Creep of Ru-Containing Nickel-Base Superalloys

2004English

Strain Induced Abnormal Grain Growth in Nickel Base Superalloys

Materials Science Forum
2013English

Multiphase Strengthened Nickel Base Superalloys Containing Refractory Carbide Dispersions

1992English

Quantitative Analysis of Gamma Prime Phase in Nickel Base Superalloys

Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan
AlloysCondensed Matter PhysicsMetalsTheoretical ChemistryMaterials ChemistryPhysical
1991English

SANS Investigation of Precipitate Microstructure in Nickel-Base Superalloys Waspaloy and DT750

English

Mechanisms of High Temperature Creep of Nickel-Base Superalloys Under Low Applied Stress

2004English

Amanote Research

Note-taking for researchers

Follow Amanote


© 2026 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy