Crack Initiation in a Coated and an Uncoated Nickel-Base Superalloy Under TMF Conditions
doi 10.1115/97-gt-236
Full Text
Open PDFAbstract
Available in full text
Date
June 2, 1997
Authors
Publisher
American Society of Mechanical Engineers