Mechanical Properties of Hydroxyapatite Single Crystals From Nanoindentation Data
Journal of the Mechanical Behavior of Biomedical Materials
- Netherlands
doi 10.1016/j.jmbbm.2010.11.001
Full Text
Open PDF
Abstract
Available in
full text
Categories
Mechanics of Materials
Biomedical Engineering
Biomaterials
Date
February 1, 2011
Authors
A. Zamiri
S. De
Publisher
Elsevier BV