Scanning Electron Microscope Observation and Surface Analysis of Oxide Films Formed on Electrical Heating Materials in the System Fe-Cr-Al at High Temperature

Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals- Japan