Development of a Third Generation DS Superalloy

doi 10.7449/2000/superalloys_2000_323_328
Full Text
Open PDF
Abstract

Available in full text

Date

January 1, 2000

Authors
T. KobayashiM. SatoY. KoizumiH. HaradaT. YamagataA. TamuraJ. Fujioka
Publisher

TMS


Related search

Development of a 4th Generation DS Superalloy

Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals
Mechanics of MaterialsAlloysMaterials ChemistryCondensed Matter PhysicsMetals
2002English

Rene' N6: Third Generation Single Crystal Superalloy

1996English

Detailed Analysis of the Solution Heat Treatment of a Third-Generation Single-Crystal Nickel-Based Superalloy CMSX-10K®

Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science
Mechanics of MaterialsAlloysCondensed Matter PhysicsMetals
2015English

Development of an Oxidation-Resistant High-Strength Sixth-Generation Single-Crystal Superalloy TMS-238

2012English

A Third-Generation Dispersion and Third-Generation Hydrogen Bonding Corrected PM6 Method: PM6-D3H+

2014English

The Third Generation

English

Production of Third-Generation Snacks

Croatian Journal of Food Science and Technology
2018English

Third-Generation Femtosecond Technology

2015English

Third-Generation Syphilis: Discussion

Sexually Transmitted Infections
DermatologyInfectious Diseases
1933English

Amanote Research

Note-taking for researchers

Follow Amanote

© 2026 Amaplex Software S.P.R.L. All rights reserved.

Privacy PolicyRefund Policy